“In an all-solid-state lithium-anode study, Mg–1 wt% La inoculation increased critical current density/capacity from 1.2 mA cm−2/0.6 mAh cm−2 for LiMg to 2.2 mA cm−2/1.1 mAh cm−2 for LiMgLa, which sustained stable plating/stripping for over 1,200 hours at 0.7 mA cm−2 at room temperature.”
2 of 4 review checks done · 1 counted · 1 by the author only
Supported · 0.9269 under ledger-default@0.3.0 at snapshot 27745 · review checks 1 of 4 · provisional until audited. The number is model-conditional, not a share of truth.
Share:
Checked in Galedra: score 0.93, strongly supported · not yet reviewed by anyone else “In an all-solid-state lithium-anode study, Mg–1 wt% La inoculation increased critical current density/capacity from 1.2 mA cm−2/0.6 mAh cm−2 for LiMg to 2.2 mA cm−2/1.1 mAh cm−2 for LiMgLa, which…” https://galedra.org/claims/6454c550-cea2-8f55-ba3f-10fd6e9d8c30/card