ClaimTypeAssessmentScoreReview checksReferences
In the reported laser-powder-bed-fused Ti–7.5Al–3.3Cr alloy, sub-10-nm hetero-stacking bands coincided with a measured yield strength of about 1.50 GPa, ultimate tensile strength of 1.73 GPa, and uniform elongation of about 7.5% in room-temperature tensile tests. QUANTITATIVE Supported 0.8808 1 of 4 93