ClaimTypeAssessmentScoreReview checksReferences
In a laboratory study of polymer–aluminum analog joints for battery interfaces, five cryogenic cooling and mild-reheating cycles reduced apparent shear strength from about 1.72 MPa untreated to 0.20 MPa after a 5-minute cooling/1-minute reheating schedule, enabling low-force separation. QUANTITATIVE Supported 0.8808 1 of 4 75