In an all-solid-state lithium-anode study, Mg–1 wt% La inoculation increased critical current density/capacity from 1.2 mA cm−2/0.6 mAh cm−2 for LiMg to 2.2 mA cm−2/1.1 mAh cm−2 for LiMgLa, which sustained stable plating/stripping for over 1,200 hours at 0.7 mA cm−2 at room temperature. QUANTITATIVE Supported 0.9269 1 of 4 114